The Modification Effects Of Cardanol

Jan 03, 2026

Leave a message

When the substitution rate reaches 15%, chemical resistance increases by 21%, and flexural strength increases by 18%.

 

At a mass fraction of 40%, the resin's elastic modulus increases by 35%.

 

The UV curing process increases the film hardness to the 2H level, and the scratch resistance is significantly better than that of thermally cured products.